C11000 Electrolytic Tough Pitch (ETP) Copper — 20 mm 3-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling C11000 Electrolytic Tough Pitch (ETP) Copper with a 20 mm 3-flute TiAlN carbide end mill, the recommended spindle speed is 3,979 RPM at 250 m/min (820.2 SFM), with a profiling feed rate of 680 mm/min (26.7 IPM) and adjusted chip load of 0.057 mm/tooth, achieving a material removal rate of 102 cm³/min (6.21 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting MathC11000 Electrolytic Tough Pitch (ETP) Copper (20 mm) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 20 mm | 10 mm | 1× | 295 | 11.6 | 59 | 1.35 |
| Slotting (100% WOC) | 3F | 20 mm | 10 mm | 1× | 443 | 17.4 | 88.6 | 2.03 |
| Slotting (100% WOC) | 4F | 20 mm | 10 mm | 1× | 590 | 23.2 | 118 | 2.7 |
| Profiling / HEM (25% WOC) | 2F | 5 mm | 30 mm | 1.1547× | 454 | 17.8 | 68.1 | 1.56 |
| Profiling / HEM (25% WOC) CURRENT | 3F | 5 mm | 30 mm | 1.1547× | 680 | 26.7 | 102 | 2.34 |
| Profiling / HEM (25% WOC) | 4F | 5 mm | 30 mm | 1.1547× | 907 | 35.7 | 136.05 | 3.12 |
| Adaptive Clearing (10% WOC) | 2F | 2 mm | 40 mm | 1.6667× | 655 | 25.8 | 52.4 | 1.2 |
| Adaptive Clearing (10% WOC) | 3F | 2 mm | 40 mm | 1.6667× | 982 | 38.7 | 78.56 | 1.8 |
| Adaptive Clearing (10% WOC) | 4F | 2 mm | 40 mm | 1.6667× | 1,310 | 51.6 | 104.8 | 2.4 |
Shop-Floor Machining Strategy for C11000 Electrolytic Tough Pitch (ETP) Copper
Work Hardening: ModerateAbundant Flood Coolant with High Lubricity Emulsion or Mineral Oil
Pressure: Flood at 8 bar minimum
Pure copper is notoriously gummy; lubrication is mandatory to prevent cold welding to cutter flutes.
Chip Flow: Long, ductile continuous ribbons. Large 1-flute or 2-flute mirror-polished end mills are required.
Milling Direction: Climb milling with high positive rake angles.
- Use polished uncoated carbide designed for aluminum/non-ferrous; razor sharp cutting edges are mandatory.
- Keep feed rate positive to shear rather than plow or smear the copper grain structure.
- Program chamfering passes immediately following roughing before secondary operations.
Frequently Asked CNC Questions (C11000 Electrolytic Tough Pitch (ETP) Copper / 20 mm)
What is the recommended RPM for milling C11000 Electrolytic Tough Pitch (ETP) Copper with a 20 mm end mill?
What table feed rate and chip load should I program for 20 mm in C11000 Electrolytic Tough Pitch (ETP) Copper?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining C11000 Electrolytic Tough Pitch (ETP) Copper?