Ti-6Al-4V Titanium Alloy (Grade 5) — 3/16" (0.1875 in) 4-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 3/16" (0.1875 in) 4-flute TiAlN carbide end mill, the recommended spindle speed is 4,345 RPM at 65 m/min (213.3 SFM), with a profiling feed rate of 224 mm/min (8.9 IPM) and adjusted chip load of 0.0129 mm/tooth, achieving a material removal rate of 1.9 cm³/min (0.12 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting MathTi-6Al-4V Titanium Alloy (Grade 5) (3/16" (0.1875 in)) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 4.76 mm | 2.38 mm | 1× | 73 | 2.9 | 0.83 | 0.05 |
| Slotting (100% WOC) | 3F | 4.76 mm | 2.38 mm | 1× | 109 | 4.3 | 1.23 | 0.07 |
| Slotting (100% WOC) | 4F | 4.76 mm | 2.38 mm | 1× | 146 | 5.7 | 1.65 | 0.1 |
| Profiling / HEM (25% WOC) | 2F | 1.19 mm | 7.14 mm | 1.1549× | 112 | 4.4 | 0.95 | 0.06 |
| Profiling / HEM (25% WOC) | 3F | 1.19 mm | 7.14 mm | 1.1549× | 168 | 6.6 | 1.43 | 0.08 |
| Profiling / HEM (25% WOC) CURRENT | 4F | 1.19 mm | 7.14 mm | 1.1549× | 224 | 8.9 | 1.9 | 0.11 |
| Adaptive Clearing (10% WOC) | 2F | 0.48 mm | 9.52 mm | 1.6608× | 162 | 6.3 | 0.74 | 0.04 |
| Adaptive Clearing (10% WOC) | 3F | 0.48 mm | 9.52 mm | 1.6608× | 242 | 9.5 | 1.11 | 0.06 |
| Adaptive Clearing (10% WOC) | 4F | 0.48 mm | 9.52 mm | 1.6608× | 323 | 12.7 | 1.48 | 0.09 |
Shop-Floor Machining Strategy for Ti-6Al-4V Titanium Alloy (Grade 5)
Work Hardening: HighHigh-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI)
Pressure: 70 bar through-spindle coolant mandatory for deep milling
Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.
Chip Flow: Chips weld chemically to tool steel and carbide at elevated temperatures.
Milling Direction: Strict climb milling. Keep radial engagement (ae) under 20% of tool diameter.
- LOW SPEED, HIGH FEED, ABUNDANT COOLANT: The universal titanium triad.
- Arc into cuts using a roll-in programmed entry; linear plunges cause tool shock fractures.
- Never dwell in the cut; program corner deceleration cautiously to prevent tool rubbing.
Frequently Asked CNC Questions (Ti-6Al-4V Titanium Alloy (Grade 5) / 3/16" (0.1875 in))
What is the recommended RPM for milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 3/16" (0.1875 in) end mill?
What table feed rate and chip load should I program for 3/16" (0.1875 in) in Ti-6Al-4V Titanium Alloy (Grade 5)?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining Ti-6Al-4V Titanium Alloy (Grade 5)?
Recent Calculations
No recent calculations saved yet.