Skip to calculator
⚙️
TorqueAndFeed TorqueAndFeed.com • B2B Reference

Ti-6Al-4V Titanium Alloy (Grade 5) — 1/4" (0.250 in) 3-Flute Speeds & Feeds

ISO Group S 330 HB / 36 HRC

Live CNC Milling Parameter Engine

24,000 RPM
mm
mm
m/min
Spindle Speed RPM
3,258 RPM
Surface Speed: 65 m/min (213.3 SFM)
Table Feed Rate F = RPM·z·fz
158 mm/min
6.3 IPM
Plunge/Ramp Rate: 55 mm/min
Adjusted Chip Load CTF: 1.1541×
0.0162 mm/t
0.00064 in/tooth
Thinning compensation applied for light stepover
Material Removal & Power MRR
2.39 cm³/min
0.15 in³/min
Power Required: 0.14 kW (0.19 HP)
Direct CNC Machining Solution

For milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 1/4" (0.250 in) 3-flute TiAlN carbide end mill, the recommended spindle speed is 3,258 RPM at 65 m/min (213.3 SFM), with a profiling feed rate of 158 mm/min (6.3 IPM) and adjusted chip load of 0.0162 mm/tooth, achieving a material removal rate of 2.39 cm³/min (0.15 in³/min).

Radial Engagement & Chip Thinning Blueprint

DIN 6584 / Sandvik
Ti-6Al-4V Titanium Alloy (Grade 5) Stock CLIMB D = 6.35 mm (0.25") ae = 1.59 mm ap = 9.52 mm Workpiece
Radial Ratio (ae/D) 25%
Chip Thinning (CTF) 1.1541×
Spindle Torque 0.32 N·m

Step-by-Step Machining Physics Proof

DIN 6584 Cutting Math
Step 1: Spindle RPM from Cutting Speed (Vc)
RPM = (Vc × 1000) / (π × D)
RPM = (65 × 1000) / (π × 6.35) = 3,258 RPM
Step 2: Radial Chip Thinning Factor (CTF)
CTF = 1 / √(1 − (1 − 2·(ae/D))²)
ae/D = 1.59/6.35 = 0.25 → CTF = 1.1541×
Step 3: Adjusted Chip Load (fz,adj)
fz,adj = fz,base × CTF
fz,adj = 0.014 mm × 1.1541 = 0.0162 mm/tooth
Step 4: Table Feed Rate (F)
F = RPM × z × fz,adj
F = 3,258 × 3 × 0.0162 = 158 mm/min (6.3 IPM)
Step 5: Material Removal Rate (MRR)
MRR = (ap × ae × F) / 1000
MRR = (9.52 × 1.59 × 158) / 1000 = 2.39 cm³/min (0.15 in³/min)
Specific Cutting Force (kc) for Ti-6Al-4V Titanium Alloy (Grade 5): 2800 N/mm². Spindle drive efficiency η = 0.80.

Ti-6Al-4V Titanium Alloy (Grade 5) (1/4" (0.250 in)) Cutting Strategy Matrix

Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).

Tool: 1/4" (0.250 in)
Operation Strategy Flutes Stepover (ae) Depth (ap) CTF Feed (mm/min) Feed (IPM) MRR (cm³/min) Power (kW)
Slotting (100% WOC) 2F 6.35 mm 3.17 mm 1× 68 2.7 1.37 0.08
Slotting (100% WOC) 3F 6.35 mm 3.17 mm 1× 103 4 2.07 0.12
Slotting (100% WOC) 4F 6.35 mm 3.17 mm 1× 137 5.3 2.76 0.16
Profiling / HEM (25% WOC) 2F 1.59 mm 9.52 mm 1.1541× 106 4.2 1.6 0.09
Profiling / HEM (25% WOC) CURRENT 3F 1.59 mm 9.52 mm 1.1541× 158 6.3 2.39 0.14
Profiling / HEM (25% WOC) 4F 1.59 mm 9.52 mm 1.1541× 211 8.3 3.19 0.19
Adaptive Clearing (10% WOC) 2F 0.64 mm 12.7 mm 1.6609× 152 6 1.24 0.07
Adaptive Clearing (10% WOC) 3F 0.64 mm 12.7 mm 1.6609× 228 9 1.85 0.11
Adaptive Clearing (10% WOC) 4F 0.64 mm 12.7 mm 1.6609× 304 12 2.47 0.14

Shop-Floor Machining Strategy for Ti-6Al-4V Titanium Alloy (Grade 5)

Work Hardening: High
Coolant & Lubrication Protocol

High-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI)

Pressure: 70 bar through-spindle coolant mandatory for deep milling

Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.

Chip Evacuation & Tool Path Guidance

Chip Flow: Chips weld chemically to tool steel and carbide at elevated temperatures.

Milling Direction: Strict climb milling. Keep radial engagement (ae) under 20% of tool diameter.

Expert Machinist Tips:
  • LOW SPEED, HIGH FEED, ABUNDANT COOLANT: The universal titanium triad.
  • Arc into cuts using a roll-in programmed entry; linear plunges cause tool shock fractures.
  • Never dwell in the cut; program corner deceleration cautiously to prevent tool rubbing.

Frequently Asked CNC Questions (Ti-6Al-4V Titanium Alloy (Grade 5) / 1/4" (0.250 in))

What is the recommended RPM for milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 1/4" (0.250 in) end mill?
For a 1/4" (0.250 in) (6.35 mm) TiAlN coated carbide end mill in Ti-6Al-4V Titanium Alloy (Grade 5), the baseline surface cutting speed is 65 m/min (213.3 SFM), which translates to a calculated spindle speed of 3,258 RPM. If using uncoated carbide, reduce surface speed to 50 m/min (165 SFM / 2506 RPM). For HSS cutters, speed must be restricted to 11 m/min (551 RPM) to avoid thermal edge failure.
What table feed rate and chip load should I program for 1/4" (0.250 in) in Ti-6Al-4V Titanium Alloy (Grade 5)?
At 3,258 RPM with a 3-flute cutter in standard 25% radial profiling engagement, the adjusted chip load is 0.0162 mm/tooth (0.00064"/tooth) after applying a radial chip thinning factor (CTF) of 1.1541×. This yields a table feed rate of 158 mm/min (6.3 IPM). Ramping or plunging into material should be limited to 35% of table feed (55 mm/min / 2.2 IPM) at an entry ramp angle of 2.5°.
Why does radial chip thinning occur when milling at less than 50% stepover?
When the radial width of cut (ae) is less than 50% of the cutter diameter, the cutting tooth leaves the cut before reaching maximum chip thickness. Without compensation, the effective chip becomes paper-thin, causing the cutter to rub and work-harden rather than shear cleanly. At 25% stepover (ae = 1.59 mm), the Chip Thinning Factor is 1.1541×, requiring a programmed feed increase to maintain the true physical chip thickness and preserve tool life.
What coolant strategy is recommended for CNC machining Ti-6Al-4V Titanium Alloy (Grade 5)?
High-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI). Pressure specification: 70 bar through-spindle coolant mandatory for deep milling. Engineering rationale: Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.