Ti-6Al-4V Titanium Alloy (Grade 5) — 3/4" (0.750 in) 4-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 3/4" (0.750 in) 4-flute TiAlN carbide end mill, the recommended spindle speed is 1,086 RPM at 65 m/min (213.3 SFM), with a profiling feed rate of 169 mm/min (6.7 IPM) and adjusted chip load of 0.039 mm/tooth, achieving a material removal rate of 22.99 cm³/min (1.41 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting MathTi-6Al-4V Titanium Alloy (Grade 5) (3/4" (0.750 in)) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 19.05 mm | 9.53 mm | 1× | 55 | 2.2 | 9.99 | 0.58 |
| Slotting (100% WOC) | 3F | 19.05 mm | 9.53 mm | 1× | 83 | 3.3 | 15.07 | 0.88 |
| Slotting (100% WOC) | 4F | 19.05 mm | 9.53 mm | 1× | 110 | 4.3 | 19.97 | 1.16 |
| Profiling / HEM (25% WOC) | 2F | 4.76 mm | 28.58 mm | 1.1549× | 85 | 3.3 | 11.56 | 0.67 |
| Profiling / HEM (25% WOC) | 3F | 4.76 mm | 28.58 mm | 1.1549× | 127 | 5 | 17.28 | 1.01 |
| Profiling / HEM (25% WOC) CURRENT | 4F | 4.76 mm | 28.58 mm | 1.1549× | 169 | 6.7 | 22.99 | 1.34 |
| Adaptive Clearing (10% WOC) | 2F | 1.91 mm | 38.1 mm | 1.6647× | 122 | 4.8 | 8.88 | 0.52 |
| Adaptive Clearing (10% WOC) | 3F | 1.91 mm | 38.1 mm | 1.6647× | 183 | 7.2 | 13.32 | 0.78 |
| Adaptive Clearing (10% WOC) | 4F | 1.91 mm | 38.1 mm | 1.6647× | 245 | 9.6 | 17.83 | 1.04 |
Shop-Floor Machining Strategy for Ti-6Al-4V Titanium Alloy (Grade 5)
Work Hardening: HighHigh-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI)
Pressure: 70 bar through-spindle coolant mandatory for deep milling
Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.
Chip Flow: Chips weld chemically to tool steel and carbide at elevated temperatures.
Milling Direction: Strict climb milling. Keep radial engagement (ae) under 20% of tool diameter.
- LOW SPEED, HIGH FEED, ABUNDANT COOLANT: The universal titanium triad.
- Arc into cuts using a roll-in programmed entry; linear plunges cause tool shock fractures.
- Never dwell in the cut; program corner deceleration cautiously to prevent tool rubbing.
Frequently Asked CNC Questions (Ti-6Al-4V Titanium Alloy (Grade 5) / 3/4" (0.750 in))
What is the recommended RPM for milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 3/4" (0.750 in) end mill?
What table feed rate and chip load should I program for 3/4" (0.750 in) in Ti-6Al-4V Titanium Alloy (Grade 5)?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining Ti-6Al-4V Titanium Alloy (Grade 5)?