Skip to calculator
⚙️
TorqueAndFeed TorqueAndFeed.com • B2B Reference

Ti-6Al-4V Titanium Alloy (Grade 5) — 1" (1.000 in) 2-Flute Speeds & Feeds

ISO Group S 330 HB / 36 HRC

Live CNC Milling Parameter Engine

24,000 RPM
mm
mm
m/min
Spindle Speed RPM
815 RPM
Surface Speed: 65 m/min (213.3 SFM)
Table Feed Rate F = RPM·z·fz
80 mm/min
3.2 IPM
Plunge/Ramp Rate: 28 mm/min
Adjusted Chip Load CTF: 1.1547×
0.0492 mm/t
0.00194 in/tooth
Thinning compensation applied for light stepover
Material Removal & Power MRR
19.35 cm³/min
1.2 in³/min
Power Required: 1.13 kW (1.51 HP)
Direct CNC Machining Solution

For milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 1" (1.000 in) 2-flute TiAlN carbide end mill, the recommended spindle speed is 815 RPM at 65 m/min (213.3 SFM), with a profiling feed rate of 80 mm/min (3.2 IPM) and adjusted chip load of 0.0492 mm/tooth, achieving a material removal rate of 19.35 cm³/min (1.2 in³/min).

Radial Engagement & Chip Thinning Blueprint

DIN 6584 / Sandvik
Ti-6Al-4V Titanium Alloy (Grade 5) Stock CLIMB D = 25.4 mm (1") ae = 6.35 mm ap = 38.1 mm Workpiece
Radial Ratio (ae/D) 25%
Chip Thinning (CTF) 1.1547×
Spindle Torque 10.54 N·m

Step-by-Step Machining Physics Proof

DIN 6584 Cutting Math
Step 1: Spindle RPM from Cutting Speed (Vc)
RPM = (Vc × 1000) / (π × D)
RPM = (65 × 1000) / (π × 25.4) = 815 RPM
Step 2: Radial Chip Thinning Factor (CTF)
CTF = 1 / √(1 − (1 − 2·(ae/D))²)
ae/D = 6.35/25.4 = 0.25 → CTF = 1.1547×
Step 3: Adjusted Chip Load (fz,adj)
fz,adj = fz,base × CTF
fz,adj = 0.0426 mm × 1.1547 = 0.0492 mm/tooth
Step 4: Table Feed Rate (F)
F = RPM × z × fz,adj
F = 815 × 2 × 0.0492 = 80 mm/min (3.2 IPM)
Step 5: Material Removal Rate (MRR)
MRR = (ap × ae × F) / 1000
MRR = (38.1 × 6.35 × 80) / 1000 = 19.35 cm³/min (1.2 in³/min)
Specific Cutting Force (kc) for Ti-6Al-4V Titanium Alloy (Grade 5): 2800 N/mm². Spindle drive efficiency η = 0.80.

Ti-6Al-4V Titanium Alloy (Grade 5) (1" (1.000 in)) Cutting Strategy Matrix

Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).

Tool: 1" (1.000 in)
Operation Strategy Flutes Stepover (ae) Depth (ap) CTF Feed (mm/min) Feed (IPM) MRR (cm³/min) Power (kW)
Slotting (100% WOC) 2F 25.4 mm 12.7 mm 1× 52 2.1 16.77 0.98
Slotting (100% WOC) 3F 25.4 mm 12.7 mm 1× 78 3.1 25.16 1.47
Slotting (100% WOC) 4F 25.4 mm 12.7 mm 1× 104 4.1 33.55 1.96
Profiling / HEM (25% WOC) CURRENT 2F 6.35 mm 38.1 mm 1.1547× 80 3.2 19.35 1.13
Profiling / HEM (25% WOC) 3F 6.35 mm 38.1 mm 1.1547× 120 4.7 29.03 1.69
Profiling / HEM (25% WOC) 4F 6.35 mm 38.1 mm 1.1547× 160 6.3 38.71 2.26
Adaptive Clearing (10% WOC) 2F 2.54 mm 50.8 mm 1.6667× 116 4.6 14.97 0.87
Adaptive Clearing (10% WOC) 3F 2.54 mm 50.8 mm 1.6667× 174 6.8 22.45 1.31
Adaptive Clearing (10% WOC) 4F 2.54 mm 50.8 mm 1.6667× 231 9.1 29.81 1.74

Shop-Floor Machining Strategy for Ti-6Al-4V Titanium Alloy (Grade 5)

Work Hardening: High
Coolant & Lubrication Protocol

High-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI)

Pressure: 70 bar through-spindle coolant mandatory for deep milling

Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.

Chip Evacuation & Tool Path Guidance

Chip Flow: Chips weld chemically to tool steel and carbide at elevated temperatures.

Milling Direction: Strict climb milling. Keep radial engagement (ae) under 20% of tool diameter.

Expert Machinist Tips:
  • LOW SPEED, HIGH FEED, ABUNDANT COOLANT: The universal titanium triad.
  • Arc into cuts using a roll-in programmed entry; linear plunges cause tool shock fractures.
  • Never dwell in the cut; program corner deceleration cautiously to prevent tool rubbing.

Frequently Asked CNC Questions (Ti-6Al-4V Titanium Alloy (Grade 5) / 1" (1.000 in))

What is the recommended RPM for milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 1" (1.000 in) end mill?
For a 1" (1.000 in) (25.4 mm) TiAlN coated carbide end mill in Ti-6Al-4V Titanium Alloy (Grade 5), the baseline surface cutting speed is 65 m/min (213.3 SFM), which translates to a calculated spindle speed of 815 RPM. If using uncoated carbide, reduce surface speed to 50 m/min (165 SFM / 627 RPM). For HSS cutters, speed must be restricted to 11 m/min (138 RPM) to avoid thermal edge failure.
What table feed rate and chip load should I program for 1" (1.000 in) in Ti-6Al-4V Titanium Alloy (Grade 5)?
At 815 RPM with a 2-flute cutter in standard 25% radial profiling engagement, the adjusted chip load is 0.0492 mm/tooth (0.00194"/tooth) after applying a radial chip thinning factor (CTF) of 1.1547×. This yields a table feed rate of 80 mm/min (3.2 IPM). Ramping or plunging into material should be limited to 35% of table feed (28 mm/min / 1.1 IPM) at an entry ramp angle of 3°.
Why does radial chip thinning occur when milling at less than 50% stepover?
When the radial width of cut (ae) is less than 50% of the cutter diameter, the cutting tooth leaves the cut before reaching maximum chip thickness. Without compensation, the effective chip becomes paper-thin, causing the cutter to rub and work-harden rather than shear cleanly. At 25% stepover (ae = 6.35 mm), the Chip Thinning Factor is 1.1547×, requiring a programmed feed increase to maintain the true physical chip thickness and preserve tool life.
What coolant strategy is recommended for CNC machining Ti-6Al-4V Titanium Alloy (Grade 5)?
High-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI). Pressure specification: 70 bar through-spindle coolant mandatory for deep milling. Engineering rationale: Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.