304 Austenitic Stainless Steel (18/8) — 3/8" (0.375 in) 4-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling 304 Austenitic Stainless Steel (18/8) with a 3/8" (0.375 in) 4-flute TiAlN carbide end mill, the recommended spindle speed is 4,679 RPM at 140 m/min (459.3 SFM), with a profiling feed rate of 526 mm/min (20.8 IPM) and adjusted chip load of 0.0281 mm/tooth, achieving a material removal rate of 17.89 cm³/min (1.1 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting Math304 Austenitic Stainless Steel (18/8) (3/8" (0.375 in)) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 9.53 mm | 4.76 mm | 1× | 170 | 6.7 | 7.71 | 0.35 |
| Slotting (100% WOC) | 3F | 9.53 mm | 4.76 mm | 1× | 255 | 10.1 | 11.57 | 0.53 |
| Slotting (100% WOC) | 4F | 9.53 mm | 4.76 mm | 1× | 341 | 13.5 | 15.47 | 0.71 |
| Profiling / HEM (25% WOC) | 2F | 2.38 mm | 14.29 mm | 1.1549× | 263 | 10.4 | 8.94 | 0.41 |
| Profiling / HEM (25% WOC) | 3F | 2.38 mm | 14.29 mm | 1.1549× | 394 | 15.6 | 13.4 | 0.61 |
| Profiling / HEM (25% WOC) CURRENT | 4F | 2.38 mm | 14.29 mm | 1.1549× | 526 | 20.8 | 17.89 | 0.82 |
| Adaptive Clearing (10% WOC) | 2F | 0.95 mm | 19.05 mm | 1.6686× | 379 | 14.9 | 6.86 | 0.31 |
| Adaptive Clearing (10% WOC) | 3F | 0.95 mm | 19.05 mm | 1.6686× | 568 | 22.3 | 10.28 | 0.47 |
| Adaptive Clearing (10% WOC) | 4F | 0.95 mm | 19.05 mm | 1.6686× | 758 | 29.8 | 13.72 | 0.63 |
Shop-Floor Machining Strategy for 304 Austenitic Stainless Steel (18/8)
Work Hardening: EXTREMEHigh-Pressure Flood Coolant (10-12% Oil Concentration)
Pressure: 20 to 70 bar through-spindle preferred
Abundant coolant is required to carry away intense heat. Poor thermal conductivity means heat stays in the cut zone.
Chip Flow: Tough, stringy, work-hardened chips. Chip clearance is paramount.
Milling Direction: MANDATORY climb milling. Conventional milling rubs before shearing and work-hardens the surface to 45+ HRC.
- NEVER DWELL OR RUB: Maintain positive feed per tooth at all times. If the cutter rubs, the workpiece work-hardens instantly.
- Use unequal helix angle (variable helix) 4-flute end mills to damp out chatter harmonics.
- AlTiN or multi-layer nano-coatings provide critical barrier against built-up edge and notch wear.
Frequently Asked CNC Questions (304 Austenitic Stainless Steel (18/8) / 3/8" (0.375 in))
What is the recommended RPM for milling 304 Austenitic Stainless Steel (18/8) with a 3/8" (0.375 in) end mill?
What table feed rate and chip load should I program for 3/8" (0.375 in) in 304 Austenitic Stainless Steel (18/8)?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining 304 Austenitic Stainless Steel (18/8)?
Recent Calculations
No recent calculations saved yet.