4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) — 5/8" (0.625 in) 3-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) with a 5/8" (0.625 in) 3-flute TiAlN carbide end mill, the recommended spindle speed is 3,810 RPM at 190 m/min (623.4 SFM), with a profiling feed rate of 578 mm/min (22.7 IPM) and adjusted chip load of 0.0506 mm/tooth, achieving a material removal rate of 54.64 cm³/min (3.33 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting Math4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) (5/8" (0.625 in)) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 15.88 mm | 7.94 mm | 1× | 251 | 9.9 | 31.65 | 1.38 |
| Slotting (100% WOC) | 3F | 15.88 mm | 7.94 mm | 1× | 376 | 14.9 | 47.41 | 2.07 |
| Slotting (100% WOC) | 4F | 15.88 mm | 7.94 mm | 1× | 501 | 19.8 | 63.17 | 2.76 |
| Profiling / HEM (25% WOC) | 2F | 3.97 mm | 23.81 mm | 1.1546× | 386 | 15.2 | 36.49 | 1.6 |
| Profiling / HEM (25% WOC) CURRENT | 3F | 3.97 mm | 23.81 mm | 1.1546× | 578 | 22.7 | 54.64 | 2.39 |
| Profiling / HEM (25% WOC) | 4F | 3.97 mm | 23.81 mm | 1.1546× | 771 | 30.3 | 72.88 | 3.19 |
| Adaptive Clearing (10% WOC) | 2F | 1.59 mm | 31.75 mm | 1.6655× | 555 | 21.9 | 28.02 | 1.23 |
| Adaptive Clearing (10% WOC) | 3F | 1.59 mm | 31.75 mm | 1.6655× | 833 | 32.8 | 42.05 | 1.84 |
| Adaptive Clearing (10% WOC) | 4F | 1.59 mm | 31.75 mm | 1.6655× | 1,111 | 43.7 | 56.09 | 2.45 |
Shop-Floor Machining Strategy for 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC)
Work Hardening: Moderate-HighAir Blast for TiAlN Coated Carbide; Flood Coolant for HSS
Pressure: 6 bar air blast or 20 bar high-pressure flood
Thermal shock from erratic coolant flow causes micro-chipping of carbide cutting edges.
Chip Flow: Short curled chips form with proper feed; excellent surface finish potential.
Milling Direction: Climb milling essential to enter at thickest chip portion.
- Pre-hardened 4140 (HT) machines cleanly with rigid setups and AlTiN or TiAlN coated tooling.
- Use high-efficiency milling (HEM): 8-12% ae radial engagement with 1.5x-2.0x ap depth of cut.
- Keep tool stickout as short as possible to eliminate chatter harmonics.
Frequently Asked CNC Questions (4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) / 5/8" (0.625 in))
What is the recommended RPM for milling 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) with a 5/8" (0.625 in) end mill?
What table feed rate and chip load should I program for 5/8" (0.625 in) in 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC)?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC)?
Recent Calculations
No recent calculations saved yet.