7075-T6 Aerospace Aluminum — 3 mm 2-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling 7075-T6 Aerospace Aluminum with a 3 mm 2-flute TiAlN carbide end mill, the recommended spindle speed is 61,540 RPM at 580 m/min (1902.9 SFM), with a profiling feed rate of 2,400 mm/min (94.8 IPM) and adjusted chip load of 0.0195 mm/tooth, achieving a material removal rate of 8.1 cm³/min (0.5 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting Math7075-T6 Aerospace Aluminum (3 mm) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 3 mm | 1.5 mm | 1× | 1,551 | 61.5 | 6.98 | 0.12 |
| Slotting (100% WOC) | 3F | 3 mm | 1.5 mm | 1× | 2,326 | 92.3 | 10.47 | 0.19 |
| Slotting (100% WOC) | 4F | 3 mm | 1.5 mm | 1× | 3,102 | 123.1 | 13.96 | 0.25 |
| Profiling / HEM (25% WOC) CURRENT | 2F | 0.75 mm | 4.5 mm | 1.1547× | 2,400 | 94.8 | 8.1 | 0.14 |
| Profiling / HEM (25% WOC) | 3F | 0.75 mm | 4.5 mm | 1.1547× | 3,600 | 142.2 | 12.15 | 0.22 |
| Profiling / HEM (25% WOC) | 4F | 0.75 mm | 4.5 mm | 1.1547× | 4,800 | 189.5 | 16.2 | 0.29 |
| Adaptive Clearing (10% WOC) | 2F | 0.3 mm | 6 mm | 1.6667× | 3,471 | 136.6 | 6.25 | 0.11 |
| Adaptive Clearing (10% WOC) | 3F | 0.3 mm | 6 mm | 1.6667× | 5,206 | 204.9 | 9.37 | 0.17 |
| Adaptive Clearing (10% WOC) | 4F | 0.3 mm | 6 mm | 1.6667× | 6,942 | 273.2 | 12.5 | 0.22 |
Shop-Floor Machining Strategy for 7075-T6 Aerospace Aluminum
Work Hardening: LowFlood Coolant with 8-10% Synthetic Soluble Oil Concentration
Pressure: Standard flood (5 bar minimum)
Zinc-alloyed aluminum chips break cleaner than 6061, with superior surface finish.
Chip Flow: Excellent short crisp chips compared to 6061. Can run 3-flute tools at aggressive feeds.
Milling Direction: Climb milling gives mirror surface finishes.
- High zinc content gives higher tensile strength; chips shear off crisply.
- Maintain tool rigidity; deflection causes dimensional drift on tight aerospace tolerances.
- Ideal candidate for High-Speed Machining (HSM) with high axial depth and light radial stepover.
Frequently Asked CNC Questions (7075-T6 Aerospace Aluminum / 3 mm)
What is the recommended RPM for milling 7075-T6 Aerospace Aluminum with a 3 mm end mill?
What table feed rate and chip load should I program for 3 mm in 7075-T6 Aerospace Aluminum?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining 7075-T6 Aerospace Aluminum?
Recent Calculations
No recent calculations saved yet.