Skip to calculator
⚙️
TorqueAndFeed TorqueAndFeed.com • B2B Reference

Ti-6Al-4V Titanium Alloy (Grade 5) — 1/2" (0.500 in) 3-Flute Speeds & Feeds

ISO Group S 330 HB / 36 HRC

Live CNC Milling Parameter Engine

24,000 RPM
mm
mm
m/min
Spindle Speed RPM
1,629 RPM
Surface Speed: 65 m/min (213.3 SFM)
Table Feed Rate F = RPM·z·fz
138 mm/min
5.4 IPM
Plunge/Ramp Rate: 48 mm/min
Adjusted Chip Load CTF: 1.1553×
0.0282 mm/t
0.00111 in/tooth
Thinning compensation applied for light stepover
Material Removal & Power MRR
8.33 cm³/min
0.51 in³/min
Power Required: 0.49 kW (0.65 HP)
Direct CNC Machining Solution

For milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 1/2" (0.500 in) 3-flute TiAlN carbide end mill, the recommended spindle speed is 1,629 RPM at 65 m/min (213.3 SFM), with a profiling feed rate of 138 mm/min (5.4 IPM) and adjusted chip load of 0.0282 mm/tooth, achieving a material removal rate of 8.33 cm³/min (0.51 in³/min).

Radial Engagement & Chip Thinning Blueprint

DIN 6584 / Sandvik
Ti-6Al-4V Titanium Alloy (Grade 5) Stock CLIMB D = 12.7 mm (0.5") ae = 3.17 mm ap = 19.05 mm Workpiece
Radial Ratio (ae/D) 25%
Chip Thinning (CTF) 1.1553×
Spindle Torque 2.29 N·m

Step-by-Step Machining Physics Proof

DIN 6584 Cutting Math
Step 1: Spindle RPM from Cutting Speed (Vc)
RPM = (Vc × 1000) / (π × D)
RPM = (65 × 1000) / (π × 12.7) = 1,629 RPM
Step 2: Radial Chip Thinning Factor (CTF)
CTF = 1 / √(1 − (1 − 2·(ae/D))²)
ae/D = 3.17/12.7 = 0.25 → CTF = 1.1553×
Step 3: Adjusted Chip Load (fz,adj)
fz,adj = fz,base × CTF
fz,adj = 0.0244 mm × 1.1553 = 0.0282 mm/tooth
Step 4: Table Feed Rate (F)
F = RPM × z × fz,adj
F = 1,629 × 3 × 0.0282 = 138 mm/min (5.4 IPM)
Step 5: Material Removal Rate (MRR)
MRR = (ap × ae × F) / 1000
MRR = (19.05 × 3.17 × 138) / 1000 = 8.33 cm³/min (0.51 in³/min)
Specific Cutting Force (kc) for Ti-6Al-4V Titanium Alloy (Grade 5): 2800 N/mm². Spindle drive efficiency η = 0.80.

Ti-6Al-4V Titanium Alloy (Grade 5) (1/2" (0.500 in)) Cutting Strategy Matrix

Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).

Tool: 1/2" (0.500 in)
Operation Strategy Flutes Stepover (ae) Depth (ap) CTF Feed (mm/min) Feed (IPM) MRR (cm³/min) Power (kW)
Slotting (100% WOC) 2F 12.7 mm 6.35 mm 1× 60 2.3 4.84 0.28
Slotting (100% WOC) 3F 12.7 mm 6.35 mm 1× 89 3.5 7.18 0.42
Slotting (100% WOC) 4F 12.7 mm 6.35 mm 1× 119 4.7 9.6 0.56
Profiling / HEM (25% WOC) 2F 3.17 mm 19.05 mm 1.1553× 92 3.6 5.56 0.32
Profiling / HEM (25% WOC) CURRENT 3F 3.17 mm 19.05 mm 1.1553× 138 5.4 8.33 0.49
Profiling / HEM (25% WOC) 4F 3.17 mm 19.05 mm 1.1553× 184 7.2 11.11 0.65
Adaptive Clearing (10% WOC) 2F 1.27 mm 25.4 mm 1.6667× 133 5.2 4.29 0.25
Adaptive Clearing (10% WOC) 3F 1.27 mm 25.4 mm 1.6667× 199 7.8 6.42 0.37
Adaptive Clearing (10% WOC) 4F 1.27 mm 25.4 mm 1.6667× 265 10.4 8.55 0.5

Shop-Floor Machining Strategy for Ti-6Al-4V Titanium Alloy (Grade 5)

Work Hardening: High
Coolant & Lubrication Protocol

High-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI)

Pressure: 70 bar through-spindle coolant mandatory for deep milling

Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.

Chip Evacuation & Tool Path Guidance

Chip Flow: Chips weld chemically to tool steel and carbide at elevated temperatures.

Milling Direction: Strict climb milling. Keep radial engagement (ae) under 20% of tool diameter.

Expert Machinist Tips:
  • LOW SPEED, HIGH FEED, ABUNDANT COOLANT: The universal titanium triad.
  • Arc into cuts using a roll-in programmed entry; linear plunges cause tool shock fractures.
  • Never dwell in the cut; program corner deceleration cautiously to prevent tool rubbing.

Frequently Asked CNC Questions (Ti-6Al-4V Titanium Alloy (Grade 5) / 1/2" (0.500 in))

What is the recommended RPM for milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 1/2" (0.500 in) end mill?
For a 1/2" (0.500 in) (12.7 mm) TiAlN coated carbide end mill in Ti-6Al-4V Titanium Alloy (Grade 5), the baseline surface cutting speed is 65 m/min (213.3 SFM), which translates to a calculated spindle speed of 1,629 RPM. If using uncoated carbide, reduce surface speed to 50 m/min (165 SFM / 1253 RPM). For HSS cutters, speed must be restricted to 11 m/min (276 RPM) to avoid thermal edge failure.
What table feed rate and chip load should I program for 1/2" (0.500 in) in Ti-6Al-4V Titanium Alloy (Grade 5)?
At 1,629 RPM with a 3-flute cutter in standard 25% radial profiling engagement, the adjusted chip load is 0.0282 mm/tooth (0.00111"/tooth) after applying a radial chip thinning factor (CTF) of 1.1553×. This yields a table feed rate of 138 mm/min (5.4 IPM). Ramping or plunging into material should be limited to 35% of table feed (48 mm/min / 1.9 IPM) at an entry ramp angle of 2.5°.
Why does radial chip thinning occur when milling at less than 50% stepover?
When the radial width of cut (ae) is less than 50% of the cutter diameter, the cutting tooth leaves the cut before reaching maximum chip thickness. Without compensation, the effective chip becomes paper-thin, causing the cutter to rub and work-harden rather than shear cleanly. At 25% stepover (ae = 3.17 mm), the Chip Thinning Factor is 1.1553×, requiring a programmed feed increase to maintain the true physical chip thickness and preserve tool life.
What coolant strategy is recommended for CNC machining Ti-6Al-4V Titanium Alloy (Grade 5)?
High-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI). Pressure specification: 70 bar through-spindle coolant mandatory for deep milling. Engineering rationale: Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.