Ti-6Al-4V Titanium Alloy (Grade 5) — 5/8" (0.625 in) 3-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 5/8" (0.625 in) 3-flute TiAlN carbide end mill, the recommended spindle speed is 1,303 RPM at 65 m/min (213.3 SFM), with a profiling feed rate of 132 mm/min (5.2 IPM) and adjusted chip load of 0.0337 mm/tooth, achieving a material removal rate of 12.48 cm³/min (0.76 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting MathTi-6Al-4V Titanium Alloy (Grade 5) (5/8" (0.625 in)) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 15.88 mm | 7.94 mm | 1× | 57 | 2.2 | 7.19 | 0.42 |
| Slotting (100% WOC) | 3F | 15.88 mm | 7.94 mm | 1× | 86 | 3.4 | 10.84 | 0.63 |
| Slotting (100% WOC) | 4F | 15.88 mm | 7.94 mm | 1× | 114 | 4.5 | 14.37 | 0.84 |
| Profiling / HEM (25% WOC) | 2F | 3.97 mm | 23.81 mm | 1.1546× | 88 | 3.5 | 8.32 | 0.49 |
| Profiling / HEM (25% WOC) CURRENT | 3F | 3.97 mm | 23.81 mm | 1.1546× | 132 | 5.2 | 12.48 | 0.73 |
| Profiling / HEM (25% WOC) | 4F | 3.97 mm | 23.81 mm | 1.1546× | 176 | 6.9 | 16.64 | 0.97 |
| Adaptive Clearing (10% WOC) | 2F | 1.59 mm | 31.75 mm | 1.6655× | 127 | 5 | 6.41 | 0.37 |
| Adaptive Clearing (10% WOC) | 3F | 1.59 mm | 31.75 mm | 1.6655× | 190 | 7.5 | 9.59 | 0.56 |
| Adaptive Clearing (10% WOC) | 4F | 1.59 mm | 31.75 mm | 1.6655× | 253 | 10 | 12.77 | 0.74 |
Shop-Floor Machining Strategy for Ti-6Al-4V Titanium Alloy (Grade 5)
Work Hardening: HighHigh-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI)
Pressure: 70 bar through-spindle coolant mandatory for deep milling
Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.
Chip Flow: Chips weld chemically to tool steel and carbide at elevated temperatures.
Milling Direction: Strict climb milling. Keep radial engagement (ae) under 20% of tool diameter.
- LOW SPEED, HIGH FEED, ABUNDANT COOLANT: The universal titanium triad.
- Arc into cuts using a roll-in programmed entry; linear plunges cause tool shock fractures.
- Never dwell in the cut; program corner deceleration cautiously to prevent tool rubbing.
Frequently Asked CNC Questions (Ti-6Al-4V Titanium Alloy (Grade 5) / 5/8" (0.625 in))
What is the recommended RPM for milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 5/8" (0.625 in) end mill?
What table feed rate and chip load should I program for 5/8" (0.625 in) in Ti-6Al-4V Titanium Alloy (Grade 5)?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining Ti-6Al-4V Titanium Alloy (Grade 5)?