4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) — 1/8" (0.125 in) 2-Flute Speeds & Feeds

ISO Group P 280-320 HB / 28-32 HRC

Live CNC Milling Parameter Engine

24,000 RPM
mm
mm
m/min
Spindle Speed RPM
19,048 RPM
Surface Speed: 190 m/min (623.4 SFM)
Table Feed Rate F = RPM·z·fz
533 mm/min
21 IPM
Plunge/Ramp Rate: 187 mm/min
Adjusted Chip Load CTF: 1.1565×
0.014 mm/t
0.00055 in/tooth
Thinning compensation applied for light stepover
Material Removal & Power MRR
2 cm³/min
0.12 in³/min
Power Required: 0.09 kW (0.12 HP)
Direct CNC Machining Solution

For milling 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) with a 1/8" (0.125 in) 2-flute TiAlN carbide end mill, the recommended spindle speed is 19,048 RPM at 190 m/min (623.4 SFM), with a profiling feed rate of 533 mm/min (21 IPM) and adjusted chip load of 0.014 mm/tooth, achieving a material removal rate of 2 cm³/min (0.12 in³/min).

Radial Engagement & Chip Thinning Blueprint

DIN 6584 / Sandvik
4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) Stock CLIMB D = 3.175 mm (0.125") ae = 0.79 mm ap = 4.76 mm Workpiece
Radial Ratio (ae/D) 25%
Chip Thinning (CTF) 1.1565×
Spindle Torque 0.04 N·m

Step-by-Step Machining Physics Proof

DIN 6584 Cutting Math
Step 1: Spindle RPM from Cutting Speed (Vc)
RPM = (Vc × 1000) / (π × D)
RPM = (190 × 1000) / (π × 3.175) = 19,048 RPM
Step 2: Radial Chip Thinning Factor (CTF)
CTF = 1 / √(1 − (1 − 2·(ae/D))²)
ae/D = 0.79/3.175 = 0.25 → CTF = 1.1565×
Step 3: Adjusted Chip Load (fz,adj)
fz,adj = fz,base × CTF
fz,adj = 0.0121 mm × 1.1565 = 0.014 mm/tooth
Step 4: Table Feed Rate (F)
F = RPM × z × fz,adj
F = 19,048 × 2 × 0.014 = 533 mm/min (21 IPM)
Step 5: Material Removal Rate (MRR)
MRR = (ap × ae × F) / 1000
MRR = (4.76 × 0.79 × 533) / 1000 = 2 cm³/min (0.12 in³/min)
Specific Cutting Force (kc) for 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC): 2100 N/mm². Spindle drive efficiency η = 0.80.

4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) (1/8" (0.125 in)) Cutting Strategy Matrix

Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).

Tool: 1/8" (0.125 in)
Operation Strategy Flutes Stepover (ae) Depth (ap) CTF Feed (mm/min) Feed (IPM) MRR (cm³/min) Power (kW)
Slotting (100% WOC) 2F 3.17 mm 1.59 mm 1× 347 13.7 1.75 0.08
Slotting (100% WOC) 3F 3.17 mm 1.59 mm 1× 520 20.6 2.62 0.11
Slotting (100% WOC) 4F 3.17 mm 1.59 mm 1× 693 27.4 3.49 0.15
Profiling / HEM (25% WOC) CURRENT 2F 0.79 mm 4.76 mm 1.1565× 533 21 2 0.09
Profiling / HEM (25% WOC) 3F 0.79 mm 4.76 mm 1.1565× 800 31.4 3.01 0.13
Profiling / HEM (25% WOC) 4F 0.79 mm 4.76 mm 1.1565× 1,067 41.9 4.01 0.18
Adaptive Clearing (10% WOC) 2F 0.32 mm 6.35 mm 1.6609× 766 30.1 1.56 0.07
Adaptive Clearing (10% WOC) 3F 0.32 mm 6.35 mm 1.6609× 1,149 45.1 2.33 0.1
Adaptive Clearing (10% WOC) 4F 0.32 mm 6.35 mm 1.6609× 1,531 60.2 3.11 0.14

Shop-Floor Machining Strategy for 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC)

Work Hardening: Moderate-High
Coolant & Lubrication Protocol

Air Blast for TiAlN Coated Carbide; Flood Coolant for HSS

Pressure: 6 bar air blast or 20 bar high-pressure flood

Thermal shock from erratic coolant flow causes micro-chipping of carbide cutting edges.

Chip Evacuation & Tool Path Guidance

Chip Flow: Short curled chips form with proper feed; excellent surface finish potential.

Milling Direction: Climb milling essential to enter at thickest chip portion.

Expert Machinist Tips:
  • Pre-hardened 4140 (HT) machines cleanly with rigid setups and AlTiN or TiAlN coated tooling.
  • Use high-efficiency milling (HEM): 8-12% ae radial engagement with 1.5x-2.0x ap depth of cut.
  • Keep tool stickout as short as possible to eliminate chatter harmonics.

Frequently Asked CNC Questions (4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) / 1/8" (0.125 in))

What is the recommended RPM for milling 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC) with a 1/8" (0.125 in) end mill?
For a 1/8" (0.125 in) (3.175 mm) TiAlN coated carbide end mill in 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC), the baseline surface cutting speed is 190 m/min (623.4 SFM), which translates to a calculated spindle speed of 19,048 RPM. If using uncoated carbide, reduce surface speed to 150 m/min (500 SFM / 15038 RPM). For HSS cutters, speed must be restricted to 24 m/min (2406 RPM) to avoid thermal edge failure.
What table feed rate and chip load should I program for 1/8" (0.125 in) in 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC)?
At 19,048 RPM with a 2-flute cutter in standard 25% radial profiling engagement, the adjusted chip load is 0.014 mm/tooth (0.00055"/tooth) after applying a radial chip thinning factor (CTF) of 1.1565×. This yields a table feed rate of 533 mm/min (21 IPM). Ramping or plunging into material should be limited to 35% of table feed (187 mm/min / 7.3 IPM) at an entry ramp angle of 3°.
Why does radial chip thinning occur when milling at less than 50% stepover?
When the radial width of cut (ae) is less than 50% of the cutter diameter, the cutting tooth leaves the cut before reaching maximum chip thickness. Without compensation, the effective chip becomes paper-thin, causing the cutter to rub and work-harden rather than shear cleanly. At 25% stepover (ae = 0.79 mm), the Chip Thinning Factor is 1.1565×, requiring a programmed feed increase to maintain the true physical chip thickness and preserve tool life.
What coolant strategy is recommended for CNC machining 4140 Chromium-Molybdenum Alloy Steel (Pre-hardened 28-32 HRC)?
Air Blast for TiAlN Coated Carbide; Flood Coolant for HSS. Pressure specification: 6 bar air blast or 20 bar high-pressure flood. Engineering rationale: Thermal shock from erratic coolant flow causes micro-chipping of carbide cutting edges.