Ti-6Al-4V Titanium Alloy (Grade 5) — 3/8" (0.375 in) 2-Flute Speeds & Feeds
Live CNC Milling Parameter Engine
For milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 3/8" (0.375 in) 2-flute TiAlN carbide end mill, the recommended spindle speed is 2,172 RPM at 65 m/min (213.3 SFM), with a profiling feed rate of 97 mm/min (3.8 IPM) and adjusted chip load of 0.0224 mm/tooth, achieving a material removal rate of 3.3 cm³/min (0.2 in³/min).
Radial Engagement & Chip Thinning Blueprint
DIN 6584 / SandvikStep-by-Step Machining Physics Proof
DIN 6584 Cutting MathTi-6Al-4V Titanium Alloy (Grade 5) (3/8" (0.375 in)) Cutting Strategy Matrix
Pre-computed Speeds & Feeds across Slotting (100% ae), Profiling (25% ae), and Adaptive/HEM (10% ae).
| Operation Strategy | Flutes | Stepover (ae) | Depth (ap) | CTF | Feed (mm/min) | Feed (IPM) | MRR (cm³/min) | Power (kW) |
|---|---|---|---|---|---|---|---|---|
| Slotting (100% WOC) | 2F | 9.53 mm | 4.76 mm | 1× | 63 | 2.5 | 2.86 | 0.17 |
| Slotting (100% WOC) | 3F | 9.53 mm | 4.76 mm | 1× | 95 | 3.7 | 4.31 | 0.25 |
| Slotting (100% WOC) | 4F | 9.53 mm | 4.76 mm | 1× | 127 | 5 | 5.76 | 0.34 |
| Profiling / HEM (25% WOC) CURRENT | 2F | 2.38 mm | 14.29 mm | 1.1549× | 97 | 3.8 | 3.3 | 0.19 |
| Profiling / HEM (25% WOC) | 3F | 2.38 mm | 14.29 mm | 1.1549× | 146 | 5.7 | 4.97 | 0.29 |
| Profiling / HEM (25% WOC) | 4F | 2.38 mm | 14.29 mm | 1.1549× | 195 | 7.6 | 6.63 | 0.39 |
| Adaptive Clearing (10% WOC) | 2F | 0.95 mm | 19.05 mm | 1.6686× | 141 | 5.6 | 2.55 | 0.15 |
| Adaptive Clearing (10% WOC) | 3F | 0.95 mm | 19.05 mm | 1.6686× | 211 | 8.3 | 3.82 | 0.22 |
| Adaptive Clearing (10% WOC) | 4F | 0.95 mm | 19.05 mm | 1.6686× | 281 | 11.1 | 5.09 | 0.3 |
Shop-Floor Machining Strategy for Ti-6Al-4V Titanium Alloy (Grade 5)
Work Hardening: HighHigh-Pressure Through-Spindle Flood Coolant (70 bar / 1000 PSI)
Pressure: 70 bar through-spindle coolant mandatory for deep milling
Titanium thermal conductivity is 1/6th of steel; heat cannot dissipate into chips and concentrates directly on the cutting edge. WARNING: Dry titanium chips present a combustible metal fire hazard.
Chip Flow: Chips weld chemically to tool steel and carbide at elevated temperatures.
Milling Direction: Strict climb milling. Keep radial engagement (ae) under 20% of tool diameter.
- LOW SPEED, HIGH FEED, ABUNDANT COOLANT: The universal titanium triad.
- Arc into cuts using a roll-in programmed entry; linear plunges cause tool shock fractures.
- Never dwell in the cut; program corner deceleration cautiously to prevent tool rubbing.
Frequently Asked CNC Questions (Ti-6Al-4V Titanium Alloy (Grade 5) / 3/8" (0.375 in))
What is the recommended RPM for milling Ti-6Al-4V Titanium Alloy (Grade 5) with a 3/8" (0.375 in) end mill?
What table feed rate and chip load should I program for 3/8" (0.375 in) in Ti-6Al-4V Titanium Alloy (Grade 5)?
Why does radial chip thinning occur when milling at less than 50% stepover?
What coolant strategy is recommended for CNC machining Ti-6Al-4V Titanium Alloy (Grade 5)?
Recent Calculations
No recent calculations saved yet.